Endura AZ25 oxygen analyzer is designed for use in processes where the temperature ranges between 600-1400°C (1112-2552°F). The probe’s robust design enables it to withstand high temperatures and reducing and sulfurous atmospheres. Supplied with a choice of protective sheath materials, the oxygen analyzer offers improved resistance to thermal stresses and shocks and highly corrosive atmospheres. This permits usage in a range of applications that are subject to sudden variations in process temperature.