Morgan Advanced Materials

The Syncarb Z2 e2 crucible was designed specifically to provide strong chemical resistance against fluxes and excellent thermal conductivity in aluminum melting and holding applications. Its high mechanical strength allows the production of much larger crucibles. Other benefits include outstanding oxidation resistance, high refractory capabilities and good thermal-shock resistance.

www.morganadvancedmaterials.com