An electrically heated cabinet oven can be used for metal-part heat-treating operations. With workspace dimensions measuring 22 inches wide x 21 inches deep x 85 inches high, the oven has 18 kW installed in Nichrome wire tubular elements to heat the oven chamber. It also features 4-inch insulated walls, an aluminized steel exterior and interior, and all safety equipment required by NFPA Standard 86 for handling flammable solvents.