CAN-ENG Furnaces International Ltd. received an order from an international mining and materials supplier for four turnkey high-temperature rotary-hearth and chain-conveyor tempering furnace systems with capacities between 10-30 tons/hour. The equipment includes the latest in energy-efficient/low-emission combustion and a state-of-the-art drive system. The systems also include atmosphere monitoring, pressure and temperature control, high-temperature cameras, safety systems and Level II automation. Start-up for each project is planned to begin in the first quarter of 2015. The customer has locations spread throughout North and South America and eastern Asia.