Diversified Services, the heat-treating division of Metal Finishing Company, completed installation of Super Systems Inc. (SSi) controls on all of its equipment. By using SSi’s 9130 controller and SuperDATA software, Diversified Services achieves accurate control of soak times, guarantees of part temperature and complete historical traceability, all of which are critical given the company’s focus on the aerospace industry. Diversified Services recently expanded its capabilities by adding vacuum furnaces and is using the SSi 9220 controller for temperature control. SSi’s 9000 Series instruments can be used for vacuum, atmosphere and nitriding applications.