EFD Induction received an order from one of Japan’s largest manufacturing companies for two Minac mobile induction heating systems. These systems will be installed at a facility in Japan and will be used for brazing generator stator bars and windings. The compact Minac features automatic electronic matching, robot compatibility and user-friendly controls. EFD Induction also received orders from two companies in India for Minac and Sinac induction heating systems. The companies, well-known names in the tool manufacturing and power-generation distribution markets, will use them for various brazing applications.The Sinac is Minac’s stationary counterpart.