Thermatool will supply a 200-kW HAZControl™ technology welder to Kubiec-Conduit, a manufacturer based in Ecuador. The two new pieces of equipment were selected for high-speed production of conduit to keep up with growing demand in South America. The welder allows the operator to select an optimal welding frequency and reliably and consistently maintain the selected power and frequency through a mill run at any given time. The Thermatool welder also has precise heat input control, resulting in the smallest id bead (uncut). These features combine to minimize scrap and maintain high-quality welds.
Thermatool to Supply Welder to Mill in Ecuador

May 29, 2014
No Comments