Solar Atmospheres of Western PA (SAWPA) has been awarded Nadcap Merit status for vacuum heat treating and brazing of metals. The successful November 2013 audit marked 10 years of doing business as a Nadcap supplier. Merit status means that SAWPA has been granted an accreditation that lasts two years, through January 2016, instead of the standard one-year accreditation.