The development of a 2400°C multipurpose vacuum furnace for laboratories and research and development facilities has been announced. The system combines high-temperature capability and process versatility. The top-loading system comes standard with a 6-inch-diameter x 6-inch-high work area, mechanical pump, gas delivery, PLC with touch-screen operator interface, multiple recipe storage, automated pump down, process alarms and safety interlocks. www.tevtechllc.com