Wall Colmonoy Ltd. has been selected by Halla Visteon Climate Control Corp. for the supply of Nicrobraz® 152 brazing paste for its new VW 1.4-liter diesel engine EGR. Specific car models for this engine include VW Polo, Seat and Skoda. This is expected to be an eight-year project. Nicrobraz 152 brazing paste was developed for use in the manufacture of exhaust gas recirculation (EGR) units and heat exchangers. Nicrobraz 152 is part of a product line of boron-free Ni-CR-Si-P filler metals that contain optimal proportions of phosphorous and silicon.