C.I. Hayes, a Gasbarre Furnace Group Company, announced the installation of a multi-zone humpback bright annealing belt furnace at a leading electronics manufacturing company in the Pacific Rim. The furnace is designed to anneal stainless steel parts to the customer’s specific thermal-profile requirements. The furnace operates at a maximum temperature of 2100°F with a dew point in the -60°F range and is equipped with a three-zone heating chamber.