Alhern-Martin Industrial Furnace Co. announced the recent installation of a continuous-belt, copper brazing andbright annealing furnace line for a multinationalautomotive supplier in Alabama. The 2,000-pound/hour brazing furnace with variable-speed atmosphere agitation cooling chambers includes an exothermic gas generator, exothermic gas dryer with dew point and hydrogen analyzers. The order included turnkey installation, commissioning and training. The new system corrected the customer’s previously existing part issues while optimizing utility efficiencies.