VFM ProgramThe new Vacuum Furnace Molybdenum Component Stocking (VFM) Program offers an expanded line of molybdenum products and services to provide vacuum-furnace customers with replacement materials for support structures, furnace rails, heat shields, heating elements, evaporation boats, crucibles and other molybdenum components. The new program includes more stock sizes and deeper inventory of molybdenum in the following forms and size ranges: rod 0.010 to 2.0 inches; sheet 0.005 to 0.187 inches; foil/coil 0.005 to 0.030 inches; plate 0.1875 to 1.00 inches; wire 0.001 to 0.125 inches; and threaded rod and hex nuts in assorted sizes. Ed Fagan Inc. offers immediate shipment of all stock materials and can cut, slit or centerless grind molybdenum to customer’s exact requirements.