Induction Tooling Inc. (ITI) of North Royalton, Ohio, received accreditation from the American Association for Laboratory Accreditation (A2LA) to ISO/IEC 17025:2005 General Requirements for Calibration and Testing Laboratories for mechanical testing of ferrous metals in their on-site metallurgical laboratory. Recognition of the metallurgical testing lab as a commercial testing facility allows ITI to support its tooling customers with validation data and testing performed to internationally recognized standards. ITI will also provide testing services to the heat-treating industry.
Induction Tooling Receives Accreditation for Mechanical Testing

December 3, 2012
No Comments