This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Durex Industries’ ceramic-heater technology offers
significant advantages over metal-based sheath heaters that have limitations in
thermal performance or material compatibility.
Ceramic Heaters
Durex Industries’ ceramic-heater technology, which is
available in either aluminum nitride (AlN) or alumina (Al2O3), offers significant
advantages over metal-based sheath heaters that have limitations in thermal
performance or material compatibility. Durex’s ceramic heaters can operate in
atmospheric and vacuum environments up to 1652°F (900°C). With its excellent
thermal efficiency, AlN heaters can be designed with a multi-layer construction
that can deliver up to 2,000 W/in2. With chemical resistance to most
acidic and alkaline solutions, these compact heaters are an ideal solution for
demanding thermal applications. Ceramic heaters can be custom-designed to
optimize thermal performance for the instrumentation or equipment’s
applications.