This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
370R REACH compliant ceramic blankets are made from alkaline
earth silicate wool and were specifically designed for use in applications that
require highly efficient thermal insulation and compliance with strict safety
requirements and regulations. 370R blankets are thermally stable to 2730°F,
flexible and resilient. They also have excellent non-wetting characteristics,
low heat storage and extremely low shrinkage. Cotronics’ REACH compliant,
high-temperature ceramic blankets are designed to replace noncompliant RCF
blankets. Applications include furnace linings, non-contaminating brazing and
sintering separators, melting furnace backup insulation, and aluminum ladle and
trough covers.