This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Graphite Metallizing Corp.
August 2, 2011
High-Temperature Bushings
GRAPHALLOY® 453 self-lubricating bushings are intended for
use in severe industrial applications where temperatures reach 750°F (400°C) or
higher. GRAPHALLOY graphite/metal alloy bushings are designed to operate
without lubrication and have proven to be successful in a variety of
high-temperature applications, including heat-treat ovens and furnaces. Among
their many advantages, GRAPHALLOY bushings operate at longer intervals without
the need for maintenance, which reduces downtime. They are an excellent choice
for applications where service and maintenance tasks are cumbersome or
difficult to perform. Additional benefits include a low coefficient of friction
and dimensional stability.