Nitrex Metal supplied an in-house nitriding system to Turbine Engineering Concepts, a provider of power-generation services. The NX-822 system, complete with Nitreg®-S potential controlled nitriding technology for stainless steels, will be capable of delivering surface treatment for custom-engineered components made of stainless steels and Inconel as well as tool steels and carbon steels. The system will also have the capability of nitriding components over 84 inches in length and will dramatically shorten delivery times for replacement parts produced by Turbine Engineering Concepts.