Deloro Stellite, a producer of wear-resistant coatings, will consolidate its U.K.-based manufacturing in Goshen, Ind. The company announced it will invest $5 million and create up to 46 new jobs by 2013. Deloro Stellite, which manufactures industrial coatings and specialty-metal castings, currently employs 60 people at its Goshen facility. The company will add a production line for rod and wire products that it is transferring from a facility in England.
Deloro Stellite is headquartered in London and manufactures coating powders and rod and wire products at 13 facilities in nine countries throughout North America, Europe and Asia. The Indiana Economic Development Corp. has offered Deloro Stellite up to $400,000 in performance-based tax credits based on the company’s job-creation plans.
Deloro Stellite to Consolidate Manufacturing in U.S.
January 13, 2011