Brazilian furnace manufacturer Metaltrend sold aluminum melting and holding furnaces for the new casting and rolling line to be installed at Novelis Brasil’s Pindamonhangaba plant. Metaltrend will supply two round top-loading melting furnaces. Each furnace is equipped with six regenerative burners and has a capacity of 140 tons. The line, which will feed a tilting holding and casting furnace, is scheduled to start up in July 2012.