No Comments
Ipsen, Inc. shipped a 2-bar TITAN® V6 to the Texas plant of a global energy company. The bottom-loading furnace, with a 60-inch x 60-inch work area, was installed by Ipsen’s field-service team. The TITAN V6 offers energy efficiency and a reduced footprint. It features an easy-to-remove hot zone and heat exchanger as well as load-proximity controls. This particular model included several standard options – all-metal hot zone, operator-access platform, 1,000-gallon backfill reservoir tank, controlled cooling using a variable-speed drive and 10-Torr hydrogen partial pressure.