This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Pyro-Paint 634-ALP is a new high-temperature ceramic coating used to insulate and seal dense refractory brick used in high-temperature furnaces and kilns to 3200°F. It can improve the reliability of the brick and protect the metal shell from corrosion. Pyro-Paint 634-ALP is an inert, chemically resistant, inorganic material that will not outgas or decompose in high-temperature corrosive applications.