SECO/WARWICK Corp. received an order from SAPA Heat Transfer for a two-chamber batch CAB brazing furnace system for its facility in Shanghai, China.
SECO/WARWICK Corp. (Meadville, Pa.; http://www.secowarwick.com) received an order from SAPA Heat Transfer for a two-chamber batch CAB brazing furnace system for its facility in Shanghai, China. The unit is a side-loading CAB furnace with a purging/cooling chamber and convection-heating chamber. The furnace is a compact design with an internal recirculation fan in the braze chamber and in the cooling chamber that uses minimal floor space. Vertically mounted heating elements and ceramic fiber thermal insulation provide reliable service in the heavy-duty furnace. The furnace is scheduled for installation in Spring 2006.