Lovejoy Inc. formed Lovejoy Sintered Technologies, a new business division also based in Downers Grove.
Lovejoy Inc. (Downers Grove, Ill.; http://www.lovejoyinc.com) formed Lovejoy Sintered Technologies, a new business division also based in Downers Grove. The new division recently installed a powder metal press that uses digital technology to measure metaled powder by weight, enabling precision measurements consistent to within ±0.04 grams, regardless of part size. Principal officers of the new division include Woodrow Haddix, president, and Jim Krecji, vice president of operations.