Alloy 330 (UNS NO8330) heat resistant alloy is an austenitic nickel-iron-chromium alloy developed to provide resistance to carburizing and oxidizing atmospheres at elevated temperatures. The addition of this material grade helps the company service the thermal processing, chemical, petrochemical and power generation industries.