This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
RA 602 CA is a nickel based heat resistant alloy offering superior strength and oxidation resistance compared to alloy 600. Due to its high strength and availability in small diameter round bar, RA 602 CA is now being utilized in vacuum heat treating applications as a means to reduce fixture weight. www.rolledalloys.com Info # 299 orwww.IHadinfo.cc
I want to hear from you. Tell me how we can improve.