This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Large titanium annealing furnace (90 in. diameter, 144 in. long) is designed to anneal military titanium parts for the F/A 22 jet fighter program. The furnace can anneal under full vacuum for flowing argon gas under partial pressure of 50 torr. This method eliminates scaling and reduces alpha case to less than 0.0005 in. www.elnik.com Info # 295 orwww.IHadinfo.cc