Universal Alloy Europe Corp., a Division of Montana Tech Components AG, chose Nitrex Metal Inc. to supply a compact nitriding system for its greenfield extrusion facility in Dumbravita, Romania. The Nitrex nitriding system is designed for a small footprint surface that allows easy implementation in the customer’s facility, which produces 7000 series hard-alloy aluminum extrusions for the aerospace market. Despite its scale, the NX-412 has a deep chamber, making it easy to load a large volume of dies weighing up to 880 pounds.
In addition, the integrated automation and Nitreg® control technology programmed for die applications will ensure process reliability and improved manufacturing productivity. Nitrex has over 250 installations in plants worldwide and has licensed its technology to heat-treating companies in Australia, Brazil, Canada, Czech Republic, France, Italy, South Korea, New Zealand, Poland, South Africa, Spain, Taiwan, Thailand, the U.K. and the U.S.
Universal Alloy Corp. Orders Nitriding System