Delta Refractories Named Unifrax Distributor
July 31, 2009
No Comments
Unifrax I LLC of Niagara Falls, N.Y., named Delta Refractories Inc. as a distributor for the Unifrax family of industrial insulation products. The new partnership couples the knowledge and expertise of Delta Refractories with Unifrax product offerings to provide quality solutions for a wide range of thermal-processing applications. Delta Refractories, which is based in Katy, Texas, is a manufacturer and distributor of a wide range of refractory maintenance materials. Established in 1971, the company serves the metals and chemical-process industries with products including blanket and textiles, pre-fired refractory shapes, die cut gaskets and vacuum-formed fiber shapes.