This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
The Therma-Panel system is designed for use in car-bottom furnace hearth refractory linings. The shapes are cast from a special type of refractory material with high impact strengths and outstanding resistance to thermal shock damage. The unique geometry of the shapes provide for stable structure while allowing no straight-through joints in the lining. Because of the independent nature of the interlocking panels, stresses are broken up and cracking is minimized.