This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
The heavy-duty HTD 4000 case-depth hardness tester allows for case depths of up to 2.8 mm to be measured by one single indentation. HTD 4000 is used to measure case depth and is capable of verifying case depths ranging from 0.4 mm up to a maximum of 2.5/2.8 mm. It utilizes a new and advanced principle based on the continuous measurement of the electrical resistance in relation to the working load applied. The design meets the demands of the heat-treatment industry. HTD 4000 is equipped with a big stand to enable the testing of large workpieces having overall dimensions up to 550 mm in height and 350 mm in depth. It is also designed for hard-to-reach areas and testing under extreme conditions.