Rolled Alloys Opens New Warehouse
March 19, 2009
No Comments
Rolled Alloys opened a 68,000-square-foot warehouse in Tulsa, Okla. The facility will inventory a full line of heat- and corrosion-resistant alloys and offer a range of processing capabilities including high-definition plasma cutting, shearing, bar sawing and gauer straightening. Rolled Alloys, which is based in Temperance, Mich., now operates facilities in Michigan, Ohio, Texas, Connecticut, California, Oklahoma, Canada, China, England, France, Germany, Italy, the Netherlands, Scotland, Singapore and Spain.
Rolled Alloys announces ZERON® 100 super duplex stainless steel to its North American inventory. ZERON 100 is a 25% chromium, 7% nickel and 3.5% molybdenum super duplex stainless steel with W and Cu additions. Rolled Alloys will carry a full product line including plate, sheet, bar, pipe, fittings and welding products.
Rolled Alloys announces ZERON® 100 super duplex stainless steel to its North American inventory. ZERON 100 is a 25% chromium, 7% nickel and 3.5% molybdenum super duplex stainless steel with W and Cu additions. Rolled Alloys will carry a full product line including plate, sheet, bar, pipe, fittings and welding products.