SECO/WARWICK has sold a traveling log-homogenizing furnace to Kaiser Aluminum Newark Works’ plant in Heath, Ohio. The system will process 2x/6x/7x alloy aluminum logs of diameters ranging from 6-29 inches. The furnace will be equipped with SECO/WARWICK’s patented adjustable airflow baffling system to control airflow distribution throughout the load and improve temperature uniformity.

SECO/WARWICK will provide the patented movable baffle design or small-load height system. This design will increase furnace performance when less than the maximum-size loads are processed. Kaiser Aluminum is a leading producer of fabricated aluminum products for aerospace, general engineering, automotive and custom industrial applications.