This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
The Series 8000 furnace is a compact, economical dual-chamber furnace. The upper chamber operates between 1850°F and 2300°F for hardening and is standard with a hearth plate to support loads up to 50 pounds per square foot of hearth area. The lower tempering chamber operates between 800°F and 1600°F and is designed with a stainless steel liner and fan to recirculate heat for uniform temperature. Both chambers are designed with multi-layered lightweight, energy-efficient firebrick and mineral wool block insulation. Quench tanks are available and can be stored below certain furnace models. Chamber sizes range from 6 inches x 6 inches x 6 inches to 24 inches x 24 inches x 48 inches.