Rolled Alloys recently acquired Clama Trade, which is located in Melegnano, Italy. Clama Trade has been a significant independent service center providing the Italian and southern European market with a wide range of expertise and inventory for over 25 years. Clama Trade’s specialty products include corrosion-resistant and high-temperature nickel-based alloys and duplex stainless steels. As part of Rolled Alloys, the company will continue operations as Clama Trade.
Clama Trade stocks its specialty products in plate, sheet, bar, flanges, fittings and welding materials. It has a 10,000-square-foot facility with access to processing equipment that permits sawing, cutting and shearing of both flat and long products.