This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
The electrically heated solution treat system was designed and manufactured for sheets of aluminum in a lab environment. The furnace has a 1.6-foot-wide x 1-foot-long x 1-foot-high basket size and a 1200°F maximum operating temperature. The equipment features a pneumatically operated quench system that provides quench time less than 3 seconds from when the doors open until the load is fully submerged. This convection furnace is constructed with 6-inch-thick can construction with 3/16-inch-thick carbon steel plate exterior and 18-gauge stainless steel interior. Handrails and ladders are included to provide access to the side-mounted and roof-mounted equipment.