This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Zenergy Power
May 7, 2008
Induction Heating System
The HTS induction heater – for just-in-time production and manufacturing of high-grade, special-alloy components – achieves an energy efficiency of over 80%, as opposed to 40-50% with conventional systems. The electromagnetic induction of eddy currents provides homogenous and precisely controllable temperature levels throughout the material. There is no risk of material damage from local overheating, and there is a very short start-up time.