This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Authentic Park products, identified by the red oval, include Polyquench 15XN, a water-based, nitrite-free polymer that deposits a lubricious, non-sticky film that precisely controls heat transfer, and washes off with water. Also: AAA Quench Oil and No. 420 (“medium hot”) quench oil provide maximum hard- ness, near-zero distortion. New! No Carb Green, a water-soluble, environmentally safe, stop-off for gas, vacuum or pack carburizing. Apply with brush, spray or immersion.