This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
RA 253 MA® is now available in round bar from Rolled Alloys. RA 253 MA is an 11% nickel and 21% chromium alloy for use up to 2000°F. Its high nitrogen content provides strength superior to 309, 310 and RA330®, while its low nickel content provides excellent economy.