This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
The F2020 Series are platinum thin-film RTD elements that are equal in accuracy to many wire-wound elements but with a much faster response. The temperature range is –70-500°C (-94-932°F), and they are available in 100, 500 and 1000 Ω configurations in Class-A, Class-B and 1/3 DIN accuracies. The actual size – 2.0 x 2.0 x 0.8 mm – make them perfect for use in tight places, and the flat profile allows for easy surface mounting.