BeaverMatic Awarded Contract from Boeing
March 29, 2007
No Comments
BeaverMatic (Rockford, Ill.) has been awarded a contract from Boeing (Portland, Ore.) to design and build an electric internal quench furnace with a load size of 30 inches wide x 48 inches deep x 20 inches high to harden 1,000-pound loads of aerospace components. This internal quench batch furnace will handle additional production requirements and will be integrated among Boeing’s previously installed BeaverMatic IQF furnace line, which includes a stationary load/unload table, washer and generator.