Aremco Products Inc.
Corr-Paint™ CP4000 is a single part, black-pigmented, ceramic-silicone based coating for protecting steel components and structures used in aircraft, automotive, chemical processing, foundry and power generation plants for applications to 1100°F. Corr-Paint™ CP4000 provides excellent adhesion to marginally prepared steel surfaces and exceptional high-temperature corrosion resistance. It is resistant to a wide range of acids, bases and solvents, and it provides good thermal shock, salt spray and UV resistance. Corr-Paint™ CP4000 dries at room temperature and cures fully during operation at temperatures above 450°F.www.aremco.com