Sheet Board Type RS-1200 is a high-strength composite designed for use as thermo-mechanical and electrical insulation in applications with temperatures as high as 2372°F (1300°C). RS-1200 is a combination of strong reinforcing fibers tightly bound in an alumina ceramic matrix, and it is completely inorganic and contains no asbestos or RCF fibers. RS-1200 exhibits greater refractoriness and homogeneity than other reinforced alumina matrix composite products and can be machined to tight tolerances with conventional carbide tooling.