This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Refractory Sheet Type RS-100 is now available in 48-inch x 48-inch boards. Refractory Sheet Type RS-100 is a fiber-reinforced structural Alumina composite with useful properties in thermal, structural and electrical insulation applications as well as in the transport of molten nonferrous metals to 2300°F.