Metal Powder Industries Foundation (MPIF), Princeton, N.J., released Machinability of Powder Metallurgy Steels by A. Salak, M. Selecka and H. Danninger.

Metal Powder Industries Foundation(MPIF), Princeton, N.J., released Machinability of Powder Metallurgy Steelsby A. Salak, M. Selecka and H. Danninger. This 536-page book aims to present knowledge concerning the machinability of powder-metallurgy steels and show areas for improvement. Because tool wear and failure result from the interaction of the workpiece, tool and cutting conditions, these areas are described and analyzed for carbon, alloyed, stainless and powder-forged steels, and sintered iron.
www.mpif.org
Info # 278 orwww.IHadinfo.cc