This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Silica Matrix Composite
April 6, 2006
ZIRCAR Refractory Composites Inc.
Refractory Sheet Type RSLE-57 is a low-expansion, high-strength reinforced silica matrix composite. The material is designed for use as a high-strength insulator in induction hot press applications. A low thermal expansion coefficient and high hot strength combine to give the material increased thermal shock resistance. The material exhibits a coefficient of expansion 0.3 °- 10-6 ºC, which provides resistance to the thermal shock up to 1200ºC (2192ºF) in an oxidizing atmosphere and permits its use with rapid variation in temperature in that zone. Beyond that temperature, it transforms into a crystalline structure while maintaining its properties up to 1650ºC (3002ºF) providing there is no significant fall in temperature. At temperatures above this, the material will exhibit surface glazing.
Report Abusive Comment