Thermetco Inc. (Montreal, Quebec) has acquired HT Tools, a simulation tool from Process-Electronic (www.process-electronic.com), to design and optimize carburizing development, replacing time-consuming calculation analysis and trails to design processes for large-scale gears. Thermetco also choose the CS 87 oxygen sensor from Process-Electronic to improve the accuracy of real-time process control of its new pit carburizing furnace.