This website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
This Website Uses Cookies By closing this message or continuing to use our site, you agree to our cookie policy. Learn MoreThis website requires certain cookies to work and uses other cookies to help you have the best experience. By visiting this website, certain cookies have already been set, which you may delete and block. By closing this message or continuing to use our site, you agree to the use of cookies. Visit our updated privacy and cookie policy to learn more.
Ionic Technologies (Greenville, S.C.) installed a plasma nitrider with 17,000-lb capacity from Rubig Technologies. It is Ionic's fourth nitriding system that employs the bi-polar pulse hot wall design. The new system uses the latest design MAP 1200 amp system. Ionic is also in the process of installing a new 10-bar VUTK design vacuum furnace from Ipsen International. The furnace has a working dimension of 40 ¥ 40 ¥ 48 and has a load capacity of 4,400 lb.