Techint Goodfellow Technologies Inc. (Mississauga, Ontario, Canada) installed and commissioned two Goodfellow EFSOP™ (Expert Furnace System Optimization Process) systems at POSCO Gwangyang Works in Korea from an order awarded by ESCO Professionals Co. Ltd. The systems are presently gathering data from the two furnaces. ESCO Professionals Co. Ltd. is an energy service company specialized in energy savings in the Korea steel industry.

www.techint-technologies.com

Info # 113 or www.IHadinfo.cc