Introducing Kanthal's newest SUPER(r) stars: four specially formulated elements that better handle specific applications and atmospheres, broadening SUPER's problem solving capabilities. The new versions are SUPER ER (oxidizing, inert and reducing atmospheres to 1600 C, or 2910 F), SUPER HT (longer life, improved form stability and rapid cycling to 1830 C, or 3325 F), SUPER RA (in reactive and reducing atmospheres, with long life to 1700 C, or 3090 F) and SUPER NC (processing with low metal content to 1800 C, or 3270 F). In addition, new Superthal(r) modules further showcase Kanthal's custom heating capabilities.